Trade Lead Description:
PROCESS OF PRODUCTION AND CHARACTER
Pink Fused Alumina is produced by doping Chromia into Alumina, which gives the material pink color. The incorporation of the Cr2O3 into the Al2O3 crystal lattice produces a slight increase in toughness and a reduced friability compared with White Fused Alumina. Compared to Brown Regular Aluminum Oxide the Pink material is harder, more aggressive and has better cutting ability. The grain shape of Pink Aluminum Oxide is sharp and angular. Applications
The FEPA F grades are especially suitable for the manufacturing vitrified bonded abrasives for working hardened steels and alloys with tensile strengths of over 50 kg/mm². It is also used in tool grinding, knife-sharpening applications, precision grinding, profile grinding, flute grinding, tooth grinding, dry grinding of blade segments and mounted wheels.
Type of Offer: |
Offer to Sell |
Quantity: |
any |
Packaging: |
Packing in 25kgs paperbags on pallets |
Price / Incoterms Conditions: |
Not Specified |
Posted from China - Henan on 26 April, 2011
|
|
|